抗倍特板施工中起泡原因怎么進(jìn)行避免?
來(lái)源:http://0473114.cn/ 日期:2021-12-09 發(fā)布人:admin
抗倍特都是由英文“Compact Laminate”音譯而來(lái),抗倍特板是由裝飾色紙含浸三聚氰胺樹(shù)脂,加上多層黑色或褐牛皮紙含浸酚醛樹(shù)脂層疊后,再用鋼板經(jīng)由高溫(150℃)高壓(1430psi)的環(huán)境壓制而成,厚度從1.6mm到25mm皆可制作。抗倍特板使用過(guò)程中有時(shí)候會(huì)出現(xiàn)起泡現(xiàn)象,那如何找到抗倍特板板起泡的原因及怎樣去解決起泡的原因呢。
Kangbeite is transliterated from "compact laminate" in English. Kangbeite plate is made of decorative colored paper impregnated with melamine resin, multi-layer black or brown kraft paper impregnated with phenolic resin, and then pressed by steel plate under high temperature (150 ℃) and high pressure (1430psi). The thickness can be made from 1.6mm to 25mm. Blistering sometimes occurs during the use of anti magnification plate. How to find the cause of blistering and how to solve it.
首先,如果起泡處挑破后現(xiàn)牛皮紙底板,則說(shuō)明所購(gòu)買(mǎi)的抗倍特板有問(wèn)題,質(zhì)量不好。如果是起泡出挑破后現(xiàn)基材,則說(shuō)明施工不成熟,為施工不當(dāng)造成的原因。下面就來(lái)介紹下導(dǎo)致抗倍特板起泡的施工原因及避免方法。
First of all, if the kraft paper bottom plate is found after the blister is broken, it indicates that the purchased anti magnification plate has a problem and the quality is not good. If the base material appears after bubbling and breaking, it indicates that the construction is immature, which is caused by improper construction. The following is to introduce the construction causes and avoidance methods of anti double plate foaming.
抗倍特板起泡的施工原因:
Construction reasons for blistering of anti magnification plate:
施工時(shí)施壓不夠,不均勻
Insufficient and uneven pressure during construction
膠水局部未干就貼合;
The glue is not dry locally;
晾置時(shí)間不夠,不均勻
The drying time is not enough and uneven
濕氣重,出現(xiàn)假干現(xiàn)象
Heavy moisture and false dryness
板材潮濕,粘不牢;
The board is wet and cannot be adhered firmly;
膠水涂刷局部過(guò)多,干不了;
Too much glue can not be applied locally;
膠水局部缺膠。
Local glue shortage.
抗倍特板起泡的避免方法;
Methods to avoid blistering of anti doubling plate;
均勻用力施壓致防火板貼合。
Apply pressure evenly to make the fireproof board fit.
適當(dāng)延長(zhǎng)晾置時(shí)間
Properly extend the drying time
通風(fēng)干燥、用太陽(yáng)燈照射或跟換場(chǎng)所;
Ventilate and dry, shine with a sun lamp or change places;
粘物晾干或烘干后再使用;
The sticky material can be used after drying or drying;
均勻、一次刮膠。
Apply glue evenly and once.
上一篇:如何判斷保溫裝飾板的質(zhì)量?
下一篇:金屬板常見(jiàn)使用解決方案
分類導(dǎo)航
Related products相關(guān)新聞
- 富美家色麗石:色麗石臺(tái)面出現(xiàn)裂紋時(shí),該如何修補(bǔ)?2024-11-16
- 你們知道富美家美耐板的優(yōu)缺點(diǎn)嗎?2024-10-18
- 富美家防火板怎么安裝施工2024-10-14
- 富美家美耐板:如何正確選購(gòu)防火板?2024-09-04
- 美耐板和三胺板的區(qū)別2024-08-22
- 富美家防火板尺寸有哪些?2024-08-05
- 富美家防火板的應(yīng)用領(lǐng)域介紹2024-08-01
- 防火板等級(jí)標(biāo)準(zhǔn)分為B1級(jí)、B2級(jí)和B3級(jí)三個(gè)等級(jí)2024-07-08
- 富美家抗倍特板的材質(zhì)是什么?2024-06-24
- 富美家抗倍特隔斷的使用特點(diǎn)2024-06-19