由于抗倍特板材的質(zhì)地很堅硬,因此在加工時應(yīng)注意相關(guān)的幾個問題,下面富美家抗倍特廠家為您分析。
Due to the hard texture of the anti-Beite plate, we should pay attention to several related problems during processing. The following is the analysis of Fumeijia anti-Beite manufacturer for you.
1.開料時,應(yīng)以直線鋸切為主。通??上仍谶@種板材上畫好規(guī)格尺寸,然后再鋸切,如果工件的尺寸為標(biāo)準(zhǔn)尺寸,可先用模板劃線,再進(jìn)行鋸切,這會方便得多。
1. During cutting, straight sawing shall be the main method. Generally, you can draw the specifications and dimensions on this kind of plate before sawing. If the size of the workpiece is standard, you can draw a line with the template before sawing, which is much more convenient.
2.開孔時,可利用手提曲線鋸進(jìn)行切割,切割速度以3-4m/min為宜,如切割速度過快,一方面會使切割邊緣產(chǎn)生爆口等缺陷,另一方面也會影響鋸條的使用壽命,增加加工成本。
2. When opening holes, the portable curve saw can be used for cutting, and the cutting speed should be 3-4 m/min. If the cutting speed is too fast, on the one hand, it will cause defects such as bursting at the cutting edge, on the other hand, it will also affect the service life of the saw blade and increase the processing cost.
3.加工異形邊沿時,應(yīng)先在板件表面劃出所需尺寸,然后利用曲線鋸切割;如果批量生產(chǎn)時,可利用模板進(jìn)行切割,這樣可確保加工速度和鋸切質(zhì)量。
3. When processing the irregular edge, the required size should be marked on the surface of the plate first, and then cut with a curve saw; In case of mass production, the template can be used for cutting, which can ensure the processing speed and sawing quality.
4.加工邊緣時,普遍采用的工具是手提鏤銑機(jī),在作業(yè)前,應(yīng)清除板件表面的灰塵或異物。以免在抗倍特板件表面留下劃痕或刻痕,鏤銑機(jī)的加工速度應(yīng)保持在2m/min為宜,如果鏤銑刀刀刃角度較小而工件厚度又較厚時,鏤銑機(jī)的加工速度應(yīng)適當(dāng)放慢。另外,銑刀刃的長度應(yīng)大于加工件的厚度,以保證一次走刀能銑削出邊緣的線型。走刀時,鏤銑刀應(yīng)從高處逐步向低處下滑直至鏤銑刀刃包容銑削邊緣。值得注意的是,走刀時,一定要保持平穩(wěn),不要讓鏤銑機(jī)晃動,晃動會使工件的邊緣形成不規(guī)則波紋,給后道砂磨拋光工序增加工作量,影響加工效率。
4. When processing edges, the commonly used tool is a portable router. Before operation, dust or foreign matters on the surface of the plate should be removed. In order to avoid leaving scratches or nicks on the surface of the anti-magnification plate, the processing speed of the router should be kept at 2 m/min. If the cutting edge angle of the router is small and the workpiece thickness is thick, the processing speed of the router should be appropriately slowed down. In addition, the length of the milling cutter edge should be greater than the thickness of the workpiece to ensure that the edge line can be milled at one time. When cutting, the router shall slide down from high to low gradually until the router edge covers the milling edge. It is worth noting that when cutting, it must be kept stable. Do not let the router shake. The shaking will cause irregular ripples on the edge of the workpiece, which will increase the workload of the subsequent sanding and polishing process and affect the processing efficiency.
以上就是相關(guān)的在處理抗倍特板時應(yīng)注意的一些問題解答了,希望給您幫助,更多相關(guān)事項就來我們網(wǎng)站http://0473114.cn咨詢吧!
The above are the answers to some questions that should be paid attention to when dealing with anti-multiplier boards. I hope to help you. Please come to our website for more relevant matters http://0473114.cn Ask!
上一篇:裝飾耐火板的三個常見問題
下一篇:裝飾耐火板的選購技巧從三個方面來看
分類導(dǎo)航
Related products相關(guān)新聞
- 富美家抗倍特:抗倍特板材成分2024-11-23
- 富美家衛(wèi)生間隔斷:隔斷板的材料該如何選擇?2024-11-21
- 富美家裝飾耐火板:耐火板單雙面該如何正確選擇?2024-11-20
- 富美家防火板:要按安裝規(guī)范標(biāo)準(zhǔn)安裝防火板2024-11-18
- 防火板和耐火板的共同點和區(qū)別2024-11-12
- 富美家防火板的優(yōu)勢2024-11-07
- 衛(wèi)生間隔斷如何選擇合適板材?2024-11-05
- 富美家防火板尺寸及應(yīng)用優(yōu)點是什么?2024-10-31
- HPL防火板和三聚氰胺板的區(qū)別2024-10-26
- 富美家抗倍特板是什么材質(zhì)2024-10-18